One-price acid recovery membrane MD
Thickness 90–120 μm, membrane resistance 0.8–1.3 Ω·cm², exchange capacity 1.5–2.3 meq/g; Smax membranes are compatible with hydrochloric acid/sulfuric acid, PD membranes uniquely recycle phosphoric acid domestically, and MD membranes are suitable for complex mixed acids; no electricity required—driven by concentration differences.
Phosphoric acid recovery membrane PD
Thickness 90–120μm, membrane resistance 0.8–1.3Ω・cm², exchange capacity 1.5–2.3meq/g; Smax membranes are compatible with hydrochloric acid/sulfuric acid, PD membranes uniquely recycle phosphoric acid domestically, and MD membranes are suitable for complex mixed acids; no electricity is required—driven solely by concentration differences.
Conventional acid recovery membrane DD
Thickness 90–120μm, membrane resistance 0.8–1.3Ω・cm², exchange capacity 1.5–2.3meq/g; Smax membranes are compatible with hydrochloric acid/sulfuric acid, PD membranes uniquely recycle phosphoric acid domestically, and MD membranes are suitable for complex mixed acids; no electricity required—driven by concentration differences.